Wire Arc Coatings In wire Arc coating, the starting wire feedstock, usually 1/16 in diameter may be composed of essentially any material that can be purchased at this size. |
|||||||||
![]() |
|||||||||
Two wires with an electrical potential are brought together at an angle of about 20 degrees. A current is drawn through the wires and they ´melt´ at their point of contact. An atomizing gas propels the molten particles at the substrate at low velocity. PTI applies about 10 different materials by this technique. |
|
|
|||||||||||||||||||||||||||||||